Sintered density - Cobalt and Cobalite®

The following curves indicate the evolution of sintered density as a function of the sintering hold temperature. 

Sintering conditions: hot press, graphite moulds, no organic binder, ramp 200°C/minute, 3 minute hold at plateau, 350 bar pressure, natural air cooling

DensityHardness | Impact Resistance